A Bord and Pillar panel is developed at a depth of 250 m in a flat coal seam. The vertical stress gradient is 0.027 MPa/m. If the strength of a square pillar is 12.5 MPa, the extraction ratio of the pillar for a safety factor of 1.5, is _____. (round off up to 2 decimals)
Min: 0.18 Max: 0.2
Answer: 0.19